Optimized Multi-Additive Formulation Balances High Compressive Strength and
A multi-parameter formulation combining an eight percent sodium alkali-activator, zero point fifty-two percent naphthalene-based superplasticizer, and zero point five percent glycol-based shrinkage-reducing agent successfully balances high mechanical performan
Illustrative imageA multi-parameter formulation combining an eight percent sodium alkali-activator, zero point fifty-two percent naphthalene-based superplasticizer, and zero point five percent glycol-based shrinkage-reducing agent successfully balances high mechanical performance with efflorescence suppression in alkali-activated slag paste, achieving an experimental twenty-eight-day compressive strength of 109.83 megapascals and a leached sodium concentration of 24.13 parts per million. Ordinary Portland cement remains the most prevalent construction material worldwide, but producing one ton of conventional cement releases approximately 0.87 tons of carbon dioxide, contributing substantially to global warming. In contrast, alkali-activated slag produced by activating ground granulated blast-furnace slag with alkaline solutions can reduce carbon dioxide emissions by forty-five to eighty percent and lower embodied energy by more than forty percent. Under alkaline conditions, the glass phase in slag depolymerizes into calcium, silicon, and aluminum tetrahedral units that condense into a dense aluminosilicate gel. Despite benefits such as rapid setting, high early-age strength, and chemical durability, alkali-activated slag typically requires ten to twenty times higher alkali concentrations than ordinary cement. This leaves abundant weakly bound sodium ions in the pore network, which readily migrate toward surfaces during moisture evaporation and react with atmospheric carbon dioxide, forming disruptive white efflorescence deposits that degrade aesthetics, impair microstructure, and compromise long-term durability.
To overcome the performance trade-offs inherent in single-variable adjustments, a research team based in China conducted a comprehensive investigation into the coupled effects of sodium alkali-activator dosage, a naphthalene-based superplasticizer, and a glycol-based shrinkage-reducing agent on the hydration kinetics, microstructural development, drying shrinkage, and efflorescence behavior of slag pastes. Ground granulated blast-furnace slag conforming to S105 grade with an irregular particle shape, a median particle diameter of 12.43 micrometers, and a chemical composition comprising 38.28 percent calcium oxide, 30.27 percent silicon dioxide, 15.83 percent aluminum oxide, and 9.68 percent magnesium oxide served as the primary precursor. Activator solutions were formulated using sodium hydroxide, commercial liquid sodium silicate, and deionized water to maintain a silicate modulus of 1.2 and a total solid content of approximately 29.0 weight percent. A commercial solid naphthalene-based superplasticizer possessing a twenty percent water-reduction capability was introduced to regulate paste fluidity, while a solid glycol-based shrinkage-reducing agent was integrated to counteract drying shrinkage. Paste specimens cast into cubic molds were subjected to standardized curing alongside accelerated exposure protocols to systematically assess how admixture interactions govern ion transport and mechanical strength.
Hydration kinetics tracked continuously over seventy-two hours via eight-channel isothermal calorimetry at twenty degrees Celsius revealed how each additive uniquely shapes reaction pathways. In binary mixtures activated solely with sodium solutions, an initial exothermic peak occurring within fifteen minutes marked precursor wetting and initial slag dissolution, followed by a primary acceleration peak between two and fifteen hours corresponding to the rapid precipitation of calcium-sodium-aluminosilicate hydrate gel. Elevating activator dosage from six to twelve percent advanced the acceleration period by thirteen hours and expanded the cumulative seventy-two-hour heat output by 30.54 percent due to enhanced alkalinity accelerating glass network depolymerization. Incorporating moderate amounts of naphthalene-based superplasticizer dispersed slag particles and improved activator contact, advancing the initial acceleration period by ten minutes at a zero point twenty-five percent dosage. However, excessive superplasticizer dosages dropped cumulative heat release by 8.82 percent at one percent dosage due to polymer adsorption on slag grains hindering continuous dissolution. Conversely, the glycol-based shrinkage-reducing agent exhibited a distinct retarding effect, delaying main exothermic peaks by up to eleven hours at two percent content because altered pore solution chemistry hindered the detachment of key calcium, silicon, and aluminum species needed to nucleate binding gels.
Mechanical testing of hardened cubic specimens conducted at three, seven, and twenty-eight days demonstrated that compressive strength exhibits contrasting responses to activator concentration and admixture levels. In the activator series prepared at a constant water-to-binder ratio of 0.40, increasing the activator dosage from six to ten percent steadily increased twenty-eight-day compressive strength from 92.73 to a peak of 108.41 megapascals, representing an improvement of 16.91 percent that aligned with enhanced cumulative heat release and gel formation. Raising the activator dosage further to twelve percent slightly diminished strength, reflecting structural disruption induced by elevated internal drying shrinkage and microcracking. In superplasticizer-modified mixtures prepared with ten percent activator, lowering the water-to-binder ratio from 0.40 to 0.38 alongside zero point five percent superplasticizer produced the highest observed twenty-eight-day compressive strength of 114.06 megapascals, representing a 5.21 percent increase over the superplasticizer-free equivalent. However, increasing the superplasticizer to one percent caused a 14.68 percent strength reduction relative to the optimal dosage due to excessive water reduction, micelle formation, and hindered slag activation. Incorporating the shrinkage-reducing agent caused a progressive decline in compressive strength across all curing ages, with a two percent dosage causing reductions of 19.63 percent at three days, 18.89 percent at seven days, and 18.45 percent at twenty-eight days due to kinetically retarded gel production.
Accelerated efflorescence evaluations performed by partially immersing the bottom two millimeters of twenty-eight-day sealed-cured prisms in deionized water for fourteen days revealed stark visual and physical variations across formulations. Digital image thresholding in ImageJ showed that increasing activator dosage from six to twelve percent expanded surface efflorescence coverage from 144.72 square millimeters to 292.56 square millimeters, covering 73.14 percent of the exposed specimen area and triggering localized peeling. This severe deposit formation stems from surplus mobile sodium ions in the pore fluid migrating upward under capillary suction and evaporation. Incorporating zero point five percent superplasticizer effectively curbed deposit formation by lowering water demand and refining internal matrix packing, though higher dosages lost this benefit due to impaired early activation. Remarkably, the shrinkage-reducing agent delivered the most pronounced visual efflorescence suppression, restricting deposit coverage to 148.68 square millimeters at a two percent dosage, representing just 37.17 percent of total surface area. Microstructural characterization using field emission scanning electron microscopy and energy-dispersive X-ray spectroscopy identified the surface deposits as well-defined rhombic crystals consisting of 14.72 weight percent carbon, 41.61 weight percent oxygen, and 43.67 weight percent sodium. X-ray diffraction patterns verified that the efflorescence consisted predominantly of sodium carbonate trihydrate, while calcium carbonate peaks were entirely absent because calcium ions remained immobilized within the binding gel network.
Ultrasonic chemical leaching evaluations using inductively coupled plasma optical emission spectrometry corroborated the visual efflorescence trends and established a direct quantitative metric for surface discoloration risk. After ten minutes of standardized ultrasonic extraction in ultrapure water, leachate sodium concentrations were consistently far higher than calcium concentrations, with the lowest observed sodium concentration of 14.52 parts per million in six percent activator paste exceeding the maximum calcium value of 9.54 parts per million found in twelve percent activator paste. A strong positive linear correlation emerged between extracted sodium concentrations and ImageJ-measured efflorescence areas, yielding a coefficient of determination of 0.726 with statistical significance below 0.001. In contrast to activator additions that increased leached sodium by 266.77 percent when moving from six to twelve percent dosage, adding zero point five percent superplasticizer reduced leached sodium by 17.36 percent compared to its control. The shrinkage-reducing agent demonstrated steady suppression of mobile alkalis, decreasing leached sodium from 30.10 to 27.55 parts per million as dosage rose to two percent. Monitoring leachate alkalinity over forty-eight hours revealed that solution pH climbed most rapidly during the first four hours, reaching 12.62 for high-alkali mixtures while remaining at 11.82 in two percent shrinkage-reducer pastes, confirming that limiting mobile ion transport restricts alkalinity release.
Mercury intrusion porosimetry and standardized length-change measurements clarified how additive combinations reorganize the internal pore architecture and govern dimensional instability. Drying shrinkage measured over twenty-eight days demonstrated extreme sensitivity to activator dosage, surging by 286.34 percent when activator levels increased from six to twelve percent due to accelerated early gel condensation and elevated capillary tension upon moisture departure. Adding zero point five percent superplasticizer reduced twenty-eight-day shrinkage by 32.8 percent relative to its activator-matched reference by lowering evaporable water content and optimizing particle packing. The glycol-based shrinkage-reducing agent achieved the most substantial dimensional control, reducing twenty-eight-day drying shrinkage by 64.49 percent at two percent dosage relative to the superplasticizer baseline by lowering pore-fluid surface tension and easing meniscus-induced capillary tensile stresses. Porosimetry data revealed that ten percent activator pastes had 53.4 percent lower total porosity than six percent activator specimens, with zero point five percent superplasticizer inducing an additional 5.9 percent porosity reduction. In contrast, adding two percent shrinkage reducer increased total porosity by seventy-nine percent to 25.69 percent, shifting pore proportions toward the 100 to 1000 nanometer range, which explains its lower compressive strength while simultaneously relieving the microscopic capillary stresses that drive cracking.
To delineate the relative importance of competing physical mechanisms governing efflorescence, researchers implemented grey relational analysis across representative mixtures designated as AA1, AA3, SP2, and SR3. The measured efflorescence area served as the reference sequence, while six experimental variables functioned as comparative sequences: the fraction of pores exceeding 1000 nanometers, pores between 100 and 1000 nanometers, pores under 100 nanometers, total porosity, twenty-eight-day drying shrinkage, and activator dosage. The resulting grey relational grades ranked in the sequence of activator dosage at 0.7992, drying shrinkage at 0.7947, large pores exceeding 1000 nanometers at 0.7534, fine pores under 100 nanometers, total porosity at 0.5808, and intermediate pores between 100 and 1000 nanometers. The relatively low correlation coefficient for total porosity indicates that overall void volume does not govern efflorescence severity on its own. Instead, efflorescence is dictated by available free sodium ions interacting with preferential migration pathways created by large macropores and drying shrinkage microcracks. Although higher activator contents refine internal gel porosity, they supply excessive unbound sodium and aggravate drying shrinkage, promoting microcracking that facilitates ion bypass. Conversely, mitigating shrinkage preserves matrix continuity and impedes advective moisture transport even when total pore volume is higher.
Synthesizing these findings into a statistical response surface methodology utilizing a seventeen-run Box-Behnken design enabled the researchers to model complex two-factor interactions and define an optimal multi-parameter formulation window. Analysis of variance conducted on fitted quadratic models for leached sodium concentration and twenty-eight-day compressive strength confirmed exceptional statistical reliability, yielding model F-values of 489.64 and 66.54, respectively, with significance probability values below 0.0001 and coefficients of determination exceeding 0.988. Main effect F-values for sodium leaching ranked activator dosage at 2717.53, shrinkage reducer at 610.98, and superplasticizer at 45.72, whereas main effect rankings for compressive strength placed the shrinkage reducer at 313.16, activator dosage at 46.67, and superplasticizer at 18.62. All two-factor interaction terms displayed probability values greater than 0.05, confirming that while independent variables did not exhibit synergistic mathematical coupling terms, their physical roles operated in tandem. Numerical multi-objective optimization performed via Design-Expert converged on an optimal mix proportion consisting of eight percent sodium alkali-activator, zero point fifty-two percent naphthalene superplasticizer, and zero point five percent shrinkage-reducing agent, designed to maximize matrix strength while curbing alkali migration.
Independent confirmation experiments executed on this optimized paste formulation validated the predictive accuracy of the response surface models, producing a measured twenty-eight-day compressive strength of 109.83 megapascals against a predicted 111.18 megapascals, representing an absolute deviation of only 1.21 percent. Similarly, experimental leached sodium concentration reached 24.13 parts per million compared to a model-predicted 23.52 parts per million, corresponding to a modest deviation of 2.59 percent and affirming the reliability of the quadratic regression framework within the investigated dosage boundaries. By coordinating activator chemistry with water-reducing and shrinkage-mitigating admixtures, the multi-parameter strategy resolves the conventional trade-off between mechanical integrity and efflorescence resistance in slag systems. Nevertheless, the authors noted that these experimental findings were derived exclusively from paste-scale specimens subjected to accelerated laboratory immersion protocols. Future research must evaluate whether these multi-additive synergies translate effectively to aggregate-filled mortar and structural concrete elements under natural weathering environments, incorporating direct microcrack tracking and long-term moisture monitoring to confirm durability under real-world construction conditions.
Subject of Research: Chemical admixture optimization for mitigating efflorescence and maintaining compressive strength in alkali-activated slag binders
Article Title: Synergistic mechanisms and mix optimization of multi‑additives for balancing efflorescence and strength in alkali‑activated slag
Article References: Wang, K., Jiang, D., Zhao, D., Liang, C., Lu, S., & Zhao, P. (2026). Synergistic mechanisms and mix optimization of multi‑additives for balancing efflorescence and strength in alkali‑activated slag. Case Studies in Construction Materials, 25, Article e06753. https://doi.org/10.1016/j.cscm.2026.e06753
Image Credits: AI Generated
DOI: 10.1016/j.cscm.2026.e06753
Keywords: alkali-activated slag, ground granulated blast-furnace slag, efflorescence, sodium carbonate hydrate, compressive strength, drying shrinkage, naphthalene-based superplasticizer, shrinkage-reducing agent, mercury intrusion porosimetry, grey relational analysis, response surface methodology, Box-Behnken design, sodium leaching, isothermal calorimetry, pore structure, low-carbon concrete, inductively coupled plasma optical emission spectrometry
News Source: Denise Maddox. (November 28, 2026). Optimized Multi-Additive Formulation Balances High Compressive Strength and Efflorescence in Alkali-Activated Slag. Scienmag.